Chlorosulfonated Polyethylene CSPE Hypalon CSM 20
CSM Rubber, Hypalon Rubber
Type
CSM 20
Chemical Properties
- CSM20 Chlorosulfonated Polyethylene rubber is off white material, ordorless evenly rubber-shape, and it has the mutual character with rubber which also has its own property.
- Chlorosulfonated Polyethylene CSM 20 is non-toxic, non-explosive, open flame burning, auto-extinction after remove.
- Hypalon Rubber CSM 20 has excellent ozone resistance, resistance to atmospheric aging, chemical resistance, better physical mechanical, thermal aging resistance and low temperature resistance (-20oC-12oC), oil resistance, flame resistance, abrasion resistance and electrical insulation etc.
Specifications
Test Item
CSM20 |
Target Values(Spec.Limits) |
Volatile(wt% less or equal) | 1.5 |
Chlorine content(wt%) | 28-32 |
Sulfur content(wt%) | 1.3-1.7 |
Mooney viscosity( ML 1+ 4 100 °C ) | 25-40 |
Application
CSM 20 Rubber can use in variety of rubber cement, adhesives specialty tapes, soft material coating natural rubber modification, synthetic rubber and some rubber products.